Advanced Technology & Materials Co., Ltd.

home products superalloys and special alloy superalloy,superalloy ingot,high temperature alloy

superalloy,superalloy ingot,high temperature alloy

Product Details:

Place of Origin Beijing, China (Mainland)
Brand Name AT&M

Payment & Shipping Terms:

Minimum Order Quantity: 100 Kilogram
Price: FOB beijing USD 5.0~100.0
Packaging Details: carton,wooden box
Delivery Time: within 30days
Payment Terms: L/C,D/A,D/P,T/T
Supply Ability: 2000.0 Metric Ton per Year

Detailed Product Description


The Fine Metal Branch of AT&M has the ability to produce master alloy bars of casting superalloys and strips of deforming superalloys,till now,we have a R&D and producing history of more than 50years in superalloy industry.

At present, we have produced the following casting master alloys: K417(IN100), K403, K4169(Inconel718C), K418(INCO713C),K640(X40),DZ40M(DSX40) etc. and the following deforming superalloys: Inconel601, Inconel800, Inconel800H, Inconel718,Rene41,Waspalloy,C263,A286,HA188,GH95 etc.

 

Product type:Fe-based superalloy,Ni-based superalloy,Co-based superalloy.

We can provide different shape products,like superalloy bar,superalloy rod,superalloy wire,superalloy ingot,superalloy strip,superalloy plate,superalloy tube,etc.

 

Superalloy is one of our main products. We have a lot of co-operating with foreign companies. Our goal is to produce superalloy materials of specification and designation needed by customers.

 

Introduction about superalloy:

 

Superalloys are important metal materials used for hot end parts of modern aerospace turbines, high temperature parts of rocket turbines and equipment in field of energy, metallurgy and chemistry. They can be used under conditions of higher stress, high temperature (600-1100) oxidization atmosphere, combustion and corrosion. According to base element, Superalloys are divided into Fe-base, Ni-base and Co-base alloys. According to formation process, superalloys are divided into deformation alloy, precision casting alloy and powder alloy. The main requirements of superalloy properties are heat-stability, heat-strength and texture stability.

 

Generally, superalloys are used in combustion chamber, force-added combustion chamber, directional blade, turbine blade and turbine disc. The typical materials used in combustion chamber and force-added combustion chamber are GH3030, GH3039, GH1140, GH333, GH2018, GH42, GH3044, GH3218, GH170, GH163 etc. Directional blade material is mainly casting alloys; the typical alloys are K32, K14, K38, K3, K5, K17, K19, K002, K20 etc. Turbine blade material is mainly age-hardening deforming alloys and casting alloys. The typical working blade material is GH4033, GH2302, GH143, GH4049, GH151, GH118, GH220, K417, K419 etc.

 

Product of ATM for example:

718

Nickel alloy precipitation hardened by gamma prime and double prime. Readily fabricated, weldable even in the hardened condition. Used for gas turbine components to 1200°F, as well as for cryogenic equipment.

 

Composition

Inventory

 

Cr

Ni

Mo

Co

Al

Ti

Other

Plate

Sheet

Bar

Welding Product

 

 

19

52

3

-

0.5

0.9

Cb: 5

X

X

X

X

 

 

 

 

Product Form

ASME

ASTM

AMS

UNS

 

 

Sheet, Plate

 

B 670

5596

 

 

 

Bar

SB-637

B 637

5662

 

 

 

Wire

 

 

5832

 

 

 


superalloy,superalloy ingot,high temperature alloy superalloy,superalloy ingot,high temperature alloy

Send your message to this supplier
« Prev Product 1 2 3 4 5 6 7 ... Next Product »

Other Products from this Supplier

Company Info

Advanced Technology & Materials Co., Ltd.
[China (Mainland)]
[Verified Member]

City: Beijing
Province/State: Beijing
Country/Region : China (Mainland)

Business Type:Manufacturer

View Contact Details

Email this page Bookmark this page Print this Page